Bev:
In past standards committee meetings (years ago no Rev D of 001 and 610), Jack Crawford made it clear there are NO requirements for voids in PTHs or some SMT components (e.g. gull wing). So if you find someone who has such you will be fortunate.
It was mentioned that soldered PTHs typically will have some voiding especially for those in years gone by who used various oils to cover the top of the wave solder reservoirs. The oil found its way into the completed wave soldered connections. Evidently there were not sufficient defects attributed to voiding to make it a broader issue. However given today's much tighter tolerances it becomes a very good question.
Gregg Owens
Technical Writer - Avionics
Space Exploration Technologies Corporation
(310) 363-6533
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Monday, May 03, 2010 12:48 PM
To: [log in to unmask]
Subject: [TN] Question about Voids in Solder Joints
TechNetters,
I was thinking about just putting "Voiding" as the e-mail title, but I
contemplated what I might get in responses and amended my title
accordingly.
My question is the following: do any of your companies have upper limits
on the amount of voiding in SMT solder joints of components that
customers have access to - like connectors and switches? These of
course are leaded components. I am not talking about Pb, but the form
of the interconnect between the component body and the board.
If so, are you willing and can you share?
Bev
RIM
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|