Victor,
We build our assemblies in panel format. This allows us to minimize handling, decrease
cycle type, and optimize throughput by performing one process on all boards on the panel
at the same time. Specific processes for which this is applicable include but are not
limited to: Screen Printing, Reflow, Wave, and Test. Since we can only place components
on one board at a time we do not see a huge savings at that step, but, we do have a savings
by not having to handle as many boards. In addition, we may simply add "rails" to boards
that we build 1-up simply for ease of handling through the SMT and Wave processes.
-Carrie
-----Original Message-----
From: Victor Hernandez [mailto:[log in to unmask]]
Sent: Thursday, August 28, 2003 10:59 AM
To: [log in to unmask]
Subject: Re: [TN] Cracking Ceramic SMT Capacitors
Carrie,
I have experience in PCB mfg. and Component Assembly. The depaneling was always done at the PCB level
not after Component Placement. Please provide more details.
Victor,
-----Original Message-----
From: Morse, Carrie [mailto:[log in to unmask]]
Sent: Thursday, August 28, 2003 8:54 AM
To: [log in to unmask]
Subject: Re: [TN] Cracking Ceramic SMT Capacitors
We have seen an increase in cracking.
The root cause for us is depanelizing using a rotary style blade cutter.
Caps and some filters too close to the edge are most subject to damage
due to the forces imparted on the board when depanelizing. Often we
can eliminate the problem by flipping the board over during depanelize, but,
that does not always work and since we do not have the tools to analyze the
forces during the depanelize process, any changes like flipping the board
over is essentially a bit of a gamble.
-Carrie
-----Original Message-----
From: Bob Perkins [mailto:[log in to unmask]]
Sent: Wednesday, August 27, 2003 7:42 PM
To: [log in to unmask]
Subject: [TN] Cracking Ceramic SMT Capacitors
Cracking Ceramic SMT Capacitors
" Is anyone else seeing an increase in the number of cracked and shorting ceramic chip capacitors? In our experience as a contract manufacturer we have, in the past, seen the occasional instance of ceramic capacitors cracking and shorting out. The cause of this problem is generally obvious, as it is isolated to components situated in areas of the PCB that are subject to flexing.
Recently however we have seen more frequent instances of this problem; very often in areas of the board that should not be experiencing any appreciable flex. Our process has not changed and neither have our sources of these components. Have chip capacitors themselves become more fragile?"
Rod Lafond
Manager, Quality Assurance and Technical Training
APEX-Micro Manufacturing Corporation
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|