     I would recommend contacting Austin American Technologies.  They 
     manufacture board and stencil cleaners and could run some tests for 
     you on their equipment with various solvents.  Contact Jon Phelps at 
     512-335-6400.
     
     As far as solvent selection goes, I would contact the manufacturer of 
     your solder paste to recommend the solvent.
     
     Make sure that the chemistry you select is compatible with the 
     equipment.
     
     Good luck.


______________________________ Reply Separator _________________________________
Subject: SMT Cleaning
Author:  [log in to unmask] at Internet
Date:    12/19/96 9:46 AM


     I'm working on developing a cleaning process for SMT.  One of the 
     challenges on the product is very low part clearances.  In many cases, 
     the devices are mounted only 1 to 3 mils from the board.  Some devices 
     also have their bodies soldered to the substrate to provide an RF 
     ground.  The substrates are ceramic, and the soldering process is IR 
     reflow.
     
     Right now we are cleaning by hand in Axarel 2200.  This is time 
     consuming and marginally effective.  I'm looking for a faster, more 
     effective process.  Any suggestions?
     
     Thanks,
     
     Kathie Lambert
     Northrop Grumman
     410-765-9746
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2