>We appreciate your Feedback Mr. Anderson, one more question, what is
>your surface prep (predip) prior to Tin plating.
>Regards / Wolfgang.

Wolfgang;

>From Nickel we have dragout rinses followed by a spray rinse, then
to a 10% sulfuric pre-dip before Tin plate. After copper plate we
also have a light microetch before the Nickel to eliminate the
possibility of peeling at the Cu/Ni interface.

Regards
George
----------------------------------------------------------------
Uvonics Co. Inc.                              [log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2