TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
David Hillman <[log in to unmask]>
Date:
Thu, 24 Feb 2000 18:09:30 -0600
Content-type:
multipart/mixed; Boundary="0__=CKS7puraFzTdF6Im1Cr14zS6gpDU4hVhSh7TfCYxsg1jK3JRY1dD10tW"
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (897 bytes) , att1.htm (931 bytes)


Hi Brent! You should be able to solder to brass - check with you flux supplier
to get their recommendations. The flux you are using may not have enough
activation to breakdown the oxides on the brass surface. On word of caution -
brass (copper and zinc alloy) can undergo 'dezincification' if there is no
barrier plating between the brass and your solder joint. In some use
environments this becomes a latent defect. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




gelon <[log in to unmask]> on 02/24/2000 04:48:15 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
      gelon <[log in to unmask]>

To:   [log in to unmask]
cc:

Subject:  [TN] brass pins



Has anyone ever tried to flow solder brass pins before? We are attempting to do
this and not having much luck. If anyone has done this before and has some
suggestions that might help I would appreciate it