All,
Thank you all for your replies. I guess I forgot to mention
that we also remove parts by fountain reflow. That would be
our preferred method of component removal. If we couldn't
remove a part with the fountain (clinched leads), our next
best method (from a PWB safety standpoint) would be
destructive removal where the leads are cut, the solder
connections reheated, the leads removed followed by wicking.
This isn't always the case with expensive military parts
where it can be cost prohibitive to destroy the part.
There was concern that pulsed solder extractors cause some
type of thermal damage to the PTH's and the opinion of the
manufacturing/assembly experts that responded was that there
is no real damage other that the possible tearing of the
barrel or pad when shearing the sweat joint.
Again, thank you all for your responses. I just needed
reassurance!!
Steve McBride
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|