Do not reflow them.
Remove, replace with a new device, bake and reball the old one, inspect it,
re-test (if practical) and then let your MRB decide what to do with it
depending on what it is going into i.e. re-use, scrap et.
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg
Sent: Wednesday, October 07, 2009 5:20 AM
To: [log in to unmask]
Subject: Re: [TN] BGA X-Ray Defect Detection Capabilities
Just out of curiosity, when you detect an open on a BGA, what do you do? I'm
suspecting it is not practical to rework just the open sj, can you reflow
the entire BGA to get the open sj to form a connection, or remove and
reattach?
Do you re-use the removed device or replace with a new one?
Is the x-ray inspection really useful, or is it just to confirm a defect
found in test? Or does it detect defects before test so that they can be
reworked prior to testing?
Is the x-ray inspection useful for getting the profile parameters correct,
and then once the process is in control the inspection no longer adds value?
Thanks,
Blair
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|