Hi guys!
I am in search for a lint-free wipe that is not like a gauze type
material. This is for the wiping the stencils after solder paste
swiping. If you could recommend a more effective material to pick up
all the solder paste waste on the stencil, please mail it to me..
Also, I would like to check if you have any line balancing softwares
that we can use. We have manual and auto process so I was wondering
if we can get a software applicable for these.
Can you also recommend a book or any reading material about the
latest in production management? I hope its available here in the
Philippines.
Thanks.
Jon Cruz
Supervising Product Engineer
Electronic Assemblies Inc.
Manila, Phillipines
e-mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|