Hi Edward,
Normally sodium carbonate, for chromic acid plating baths anyway. (250 g/l
chromic acid, 2.5 g/l sulphuric acid).
Best Regards,
Ken McGowan, Dublin.
----- Original Message -----
From: "Edward Szpruch" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, July 17, 2001 7:44 AM
Subject: [TN] Scrubber for NOx
> Hi,
> We are using nitric acid for stripping of plating racks and during this
> process some amount of NOx escapes to air.
> We have been requested by environmental authorities to install wet
scrubber
> for absorption of NOx.It seems,that diluted alkaline solution ( such as
> caustic soda ) will do the job of absorption of NOx.
> What is the common practice? I presume some of plating shops are using
> nitric acid for racks stripping.
> Best regards
> Edward
>
>
> Edward Szpruch
> Eltek , Manager of Process Engineering
> P.O.Box 159 ; 49101 Petah Tikva Israel
> Tel ++972 3 9395050 , Fax ++972 3 9309581
> e-mail [log in to unmask]
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|