Appears that you are talking about soldering metals to metals and not
soldering to electrical components. If this is true, mechanical
soldering requirements and not J-STD-001 soldering would normally apply.
Is this a soldering or otherwise a brazing operation since many heat
sinks are brazed to the copper pipes using dip braze or furnace brazed
process rather than soldered.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Thursday, August 29, 2013 3:10 PM
To: [log in to unmask]
Subject: Re: [TN] Solder joint failure
Usually a sacrificial gold is the final finish over the nickel. The
fluxes used to solder to nickel are unique. IMHO, no-cleans; not
allowed.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin
Sent: Thursday, August 29, 2013 12:01 PM
To: [log in to unmask]
Subject: Re: [TN] Solder joint failure
In my experience nickel is NOT easy to solder to at all.
-----Original Message-----
From: Victor Hernandez [mailto:[log in to unmask]]
Sent: Thursday, August 29, 2013 2:53 PM
To: [log in to unmask]
Subject: [TN] Solder joint failure
Fellow TechNetters:
Should I be concern with an electroless matted nickel plating over an
aluminum sheet metal surface and solder onto a copper heat tube? I
recall something about directly soldering onto a nickel surface. Beside
nickel oxidation. Any suggestions would be greatly appreciated.
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|