TECHNET Archives

June 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Date:
Fri, 17 Jun 2011 15:26:58 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Torsten Hagge <[log in to unmask]>
Message-ID:
Subject:
From:
Torsten Hagge <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (107 lines)
No, liable is the one who sold items with this solder, not that supermarket! And for repair it is much easier to use the SnPb solder... You have the same with some car horns, in Germany it is allowed to build in a very big ship fog horn (Tyfon) but it is not allowed to use it...

Best Regards,
Torsten

i.A. Dipl.Ing.(FH)Torsten Hagge
team leader HW development & 
tech. projectmanager
Kristronics GmbH
Gewerbegrund 5 - 9
24955 Harrislee
 
Tel.:    +49 461 7741 624
Fax:     +49 461 7741 642
[log in to unmask]
www.kristronics.de
 
Gerichtsstand Flensburg, Handelsregister: HRB 1433 FL
Geschäftsführer Dipl.-Ing. oec. Thormod Ohm
Ust-Id-Nr. DE 811182059
Bankverbindung: Deutsche Bank AG Flensburg, Konto-Nr. 4216610, BLZ 21570011
IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Phil Nutting
Gesendet: Freitag, 17. Juni 2011 15:16
An: [log in to unmask]
Betreff: Re: [TN] Sn60/Pb40 RoHS???????????

Gee, my supermarket only carries food.   You have one that sells electronic parts?  Kewl!

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Friday, June 17, 2011 8:59 AM
To: [log in to unmask]
Subject: [TN] Sn60/Pb40 RoHS???????????

This morning, the other half forced me into a supermarket run by a
German heavy discounter whose name is four letters with the first and
last one being the same.

To my astonishment, I found reels of solder wire with F-SW32 flux core
there, clearly labelled "Electronic solder". Guess what? It was
Sn60Pb40! They can't even claim it was old stock, because the store was
opened only a few months ago, the first on the island.

The solder was made in Wuppertal, Germany, noted for its monorail public
transport system, and was bright, not visibly oxidised, so I presume
reasonably freshly made.

As such solder is sold specifically as a component for electronics
assembly, is L*** on the wrong side of the RoHS Directive? If not, are
they liable if someone uses it to make an item of equipment for sale?

Brian

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender.  If you have received this email in error, please immediately return it to sender and delete the copy you received.



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2