MEK not only removes solder mask residues but the solder mask too. Depending
on the degree of "cure", MEK can reduce the trapped bubbles in solder mask
and make them into pinholes. If over traces, this could be very dangerous. It
is not recommended to use MEK.

***************************************************************************