TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, J W <[log in to unmask]>
Date:
Wed, 23 Sep 2009 14:28:46 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "McGlaughlin, Jeffrey A" <[log in to unmask]>
Subject:
From:
"McGlaughlin, Jeffrey A" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (51 lines)
Look at IPC-1710 it should be what you are looking for.  


Jeffrey A McGlaughlin, CID
Engineering Designer
Battelle
505 King Ave
Columbus Ohio 43201-2693
Phone (614)424-7582


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of J W
Sent: Wednesday, September 23, 2009 1:27 PM
To: [log in to unmask]
Subject: [TN] Abroad Printed Circuit Board supplier checklist

Hi,

Due to our recent introduction to poor quality bare board suppliers out of
China, our purchasing manager is looking for a checklist of some sort that
will assist us in qualifying new board suppliers.  I'm asking for your input
or suggestions on where I can find a checklist of items we should be looking
at when qualifying a new bare board supplier.  I have not searched the IPC
website yet, but will be looking next, does anyone know if IPC has a
qualification process already in place for bare board suppliers?  Is anyone
willing to share their list or qualification process?

Thanks,
Jim

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2