Dick Desrosiers <[log in to unmask]>
Date:
Sat, 01 Mar 1997 16:09:16 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
The environmentally unsafe problems of silver reclamation, as well as the humanly unsafe problems associated with ammonia, have been eliminated from the photo plotting process with the Dry Process Direct write systems.  The Graphics Art industry has been using the Lino-Type Hell (Heidelberg) Dry Setter photo plotter and Polaroid Dry Imagesetter film for several years now with great success, performance wise as well as environmentally and ecomocally.

I hesitate to use this forum for marketing purposes, however, not being the first to do so, I should point out that AOI International is now installing several Polaroid/Heidelberg systems in PCB shops after an extensive testing and evaluation period.

Dick Desrosiers
[log in to unmask]
[log in to unmask]
[log in to unmask]
508-937-5400  ext 212
508-441-0122 (fax)

----------
From: 	Roubineau, Pascal[SMTP:[log in to unmask]]
Sent: 	Tuesday, January 21, 1997 12:42 PM
To: 	'smtp: [log in to unmask]
Subject: 	RE: handling silver halide wastes


I've noted several posts about handling silver bearing wastes & wastewater 
and I have some comments as an industrial waste inspector that may (or may 
not) be useful:

The EPA considers wastewater from film developing to be a Printed Circuit 
Board Manufacturing process water just like the water from plating, etching, 
etc. is.  This means that you don't have to meet the federal silver limit 
until the wastewater is mixed together & being discharged, the significance 
of the legal *dilution* with non-silver bearing wastewater obviously 
depending on the volume of your other rinses.  Obviously if your 
film/artwork site is in a separate facility or you drain wastewater from 
there separately from your plating area this doesn't apply.

I'm not putting down waste minimization, far from it.  There are many cost & 
regulatory benefits to waste minimization in addition to my narrow focus of 
pollutants to the sewer.   I put in my two cents worth since previous posts 
seemed unclear on where federal silver limits would be applied, which may 
affect the business decision of what to spend on silver treatment.

Pascal Roubineau

(The opinions stated here are mine and not necessarily the same as my 
employer)

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************




***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2