TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Wed, 27 Sep 2006 15:26:08 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (189 lines)
A little bit of tack testing and plenty of information on slump test is
covered in J-STD-005 and J-STD-006, and in the TMs in 650 called out
within those documents, but probably not enough regarding the
application of the pastes.
The application is important as well, ie, if you are running a
high-speed turret-type placer the tackiness and slump qualities are much
more critical than if you are running a gantry style placer. And if you
are dealing with pitches of .8mm or less, again the ability of the paste
to form a good, clean brick without slumping is again very critical.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Wednesday, September 27, 2006 2:12 PM
To: [log in to unmask]
Subject: Re: [TN] Solder paste question

        Thanks for the correction Steve. I have seen the equipment that
does the Sipad process and talked with one of the fellows that is
pioneering that process in the USA at length. The main point, some
pastes loose their tackiness in about an hour and some last as Steve
said much longer. A test should be made to see how long does a
particular formulation keeps its tackiness and then stay within the
time. Of course the test board should be fully inspected for good solder
joints.
        Ramon
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, September 27, 2006 2:16 PM
To: [log in to unmask]
Subject: Re: [TN] Solder paste question

Solder Pastes that are tacky for weeks? I don't think so. 

SiPad is not a solder paste but a solid solder deposit that has been
flattened and then a tacky flux applied over that. Then the board is
covered with a slip sheet to keep the tacky flux reasonably fresh.


-Steve Gregory- 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Wednesday, September 27, 2006 1:00 PM
To: [log in to unmask]
Subject: Re: [TN] Solder paste question

 

        Joel:
        Some pastes can be tacky for weeks (Sipad) and some will loose
their tackiness in an hour and parts start sliding over the solder
balls, at which time parts need to be taken off the board, board cleaned
and part placement process started again. It all depends on the solder
paste formulation. Placing a board on its side will risk parts sliding
down, not recommended, unless you are using Sipad, very tacky firm
paste.
        Regards,
        Ramon


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, September 27, 2006 11:27 AM
To: [log in to unmask]
Subject: Re: [TN] Solder paste question

Hi Joel!

First off, I'm not aware of any "Industry Standard", because it's all
going to depend on the solder paste. All solder paste "slumps" to one
degree or another, depending on the formulation, environment, etc..
Personally, I wouldn't like to see a printed board set for more than an
hour or two before it was placed if you can help it...especially if
there's any fine pitch or BGA's on the board.

Saying that, there's been some unusual circumstances where I've had to
hand place boards and they've sat for eight hours before I had all the
components placed and the boards reflowed. Once or twice in another
life, it's taken more than a day to finish hand placing a board (I don't
ever want to do that again!) and getting it in the oven. Did the boards
reflow okay? Kinda'...there WAS just a little touch-up needed! (GRIN)

When you say sideways on a tray, are you talking about tilt-racks?
Because if you are, I would say that isn't a good idea. Gravity is only
going to exacerbate any slump issues that the paste experiences.

 
-Steve Gregory-



-----Original Message-----
From: TechNet [mailto:[log in to unmask] <mailto:[log in to unmask]> ] On
Behalf Of Joel Alexander
Sent: Wednesday, September 27, 2006 10:06 AM
To: [log in to unmask]
Subject: [TN] Solder paste question

Is there any industry standard on how long a printed board can sit prior
to reflow?  Also if a printed board is placed sideways on a tray, can
this cause print quality issues?



Joel Alexander

APSCO Quality Assurance Manager

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives
<http://listserv.ipc.org/archives>  Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>  for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2