Try Dupont for the FEP material - not easy to get any more - I doubt they
have your construction. Tring to bond FEP over .020 copper - I hope you have
developed some very fancy press pad makeups otherwise you will never get it
to seal.
Steve Kelly
PFC Flexible Circuits Ltd.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Hinners Hans Civ
WRALC/LYPME
Sent: Thursday, August 17, 2000 11:42 AM
To: [log in to unmask]
Subject: [TN] Need Flex Material Sources/Distributors
Hello Hello,
I need to find a some Flex Material sources.
I've made some inquiries but that I would include the list in my search.
IPC-FC-232A/3 -C1E2M13 (FEP cover layer)
IPC-CF-150, CF-W7-14N (Copper Core)
Alternate material: 0.20 strip copper QQ-C-576, temper cold-rolled soft
annealed
And for fun, ask your plating engineer/chemist if they want to plate up to
14 ounces (~19 mils) of copper? Mine freaked.
Off list, on list what ever works.
Hans
~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Materials Engineer (Process & Manufacturing)
Warner Robins Air Logistics Center
Avionics Production Division
Manufacturing Branch
380 Second Street, Suite 104
Building: 640, Mail Stop: LYPME
Robins AFB, GA 31098-1638
Voice: (478) 926 - 1970 Fax: (478) 926 - 7164
mailto:[log in to unmask]
http://www.robins.af.mil
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|