TECHNET Archives

June 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="ISO-8859-1"
Sender:
Subject:
From:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Date:
Tue, 18 Jun 2002 17:26:41 +0200
MIME-Version:
1.0
X-To:
"Kasprzak, Bill (sys) USX" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Ingemar Hernefjord (EMW)" <[log in to unmask]>
Parts/Attachments:
text/plain (57 lines)
Have been soldering like that for years, all seems to be about soldering profile (underlined!!), pad size, solder amount, board warpage and CTE matching. And, finally, length x width x thickness of cercaps seems to be key to successable soldering as well as direction of caps vs long/short sides of the board. Ain't quite straight that way, but doable. We soldermount lots of cercaps, even 2225, without cracks (at least I hope so...)
I assume you have already been reading AVX internet pages in the matter, lot's of recipes to make best ceramic pie..
Ingemar Hernefjord
Ericsson Microwave Systems

-----Original Message-----
From: Kasprzak, Bill (sys) USX [mailto:[log in to unmask]]
Sent: den 18 juni 2002 16:30
To: [log in to unmask]
Subject: [TN] Wavesoldering Ceramic Caps


Hello gang,

We have a situation where a board design has some 2225 Ceramic Caps on the
bottom side of the board. Most of the advisories I've seen indicates that
wavesoldering these parts is not recommended. From what I can gather,
thermal shock induces micro fractures within the ceramic substrate that
leads to component failure. However, I'm thinking that if I could raise my
normal wave preheat and lower my pot temperature, I could minimize the
thermal shock. I could almost have a thermal profile that would be similar
to reflow soldering. Reflow soldering of these ceramic caps, from what I've
read, is OK. Some of the articles I've read on this cracking phenomenon were
written in the late 80's, Is there any newer information out there?

Is anyone out there routinely wave soldering these parts that could give me
some pointers?

We use an OA flux with a DI water wash in our process.

As always your help is greatly appreciated.

Bill Kasprzak
Moog Inc. Manufacturing Engineering, Electronics

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2