Recently, I have found that Cu thickness plated onto panels may vary uo
to 150 u inches from one panel to another under the same conditions and
current and in the same bath.
Did I do anything wrong? I am using a Macdermid acid plating bath 9241.

My e-mail : [log in to unmask]

THANKS!!!!!!!!

Francis