TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Eric Masters <[log in to unmask]>
Date:
Fri, 1 Oct 1999 03:06:23 EDT
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (29 lines)
I'm having a rather perplexing problem with shorts on inner layers.  The
short is very small, and occurs mainly on fine line jobs (5/5 mils and less).
 It also occurs primarily on layers with one ounce copper, although I've seen
it on half ounce.

The short is very very small; in fact, it is rarely seen at AOI.  Usually, it
is discovered at final electrical test.  Failure analysis exhibits a very
fine sliver of copper that appears to have broken loose from a trace; it
remains attached at one end and flips across the adjacent circuit.

Cross sections and SEM's of both developed resist and etched layers show a
near vertical sidewall.  Has anyone seen this phenomenon?  Any suggestions?

Eric

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2