TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"Michael D. Doty" <[log in to unmask]>
Date:
Thu, 1 Apr 1999 18:34:42 -0500
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (24 lines)
     Hi Techies,
                I'm currently having a problem getting even coverage on a
     panel that has lots of smts and bgas. I run a dip process and have
     eliminated everything up to and including the entek as a problem. All
     solutions have been changed and different methods of precleaning have
     been tried. Short of conveyorized equipment is there anything that I
     can try so as to eliminate the spotty coverage.

                Thanks in advance,

                       Mike Doty

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2