My problem is dropping solder ball from BGA devices after ball attachment process.
First, I suspected the tempareture of reflow oven, but that was sufficient to melt
solder ball. After reflow, some balls(5-10% of strip) are missing, and empty pads
are not wetting or partialy wetting.
I found voids in flux on pad before placing ball, so I guess the void will expand
in reflow furnace, and ball dosen't touch to pad. I use dispensing system to provide
flux, which sometimes contaminates air void to flux on pad.
Does anyone have any experiences and suggestions to solve this problem ?

Thanks in advance.
---------------------
Fumiaki Shigeoka
[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2