TECHNET Archives

February 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 9 Feb 2011 16:57:21 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Reid <[log in to unmask]>
Subject:
From:
Paul Reid <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (91 lines)
There are about six failure modes that can occur with a four stack
microvia on a buried.

Because the microvias are stacked on a buried via pad rotation on the
microvia is up rather than down. 

There is microvia to target pad separation, corner cracks on the filled
microvia (where the fill dips down there will be a thin copper at the
knee) , copper pull out (crack around the base of the microvia on the
cap of the buried, wrap crack, cap lift and cap crack just beside the
knee of the buried via.

Tell us that this is a lead free application.




Sincerely, 
Paul Reid 

Program Coordinator 
PWB Interconnect Solutions Inc. 
235 Stafford Rd., West, Unit 103 
Nepean, Ontario 
Canada, K2H 9C1 
613 596 4244 ext. 229 
Skype paul_reid_pwb 
[log in to unmask] <mailto:[log in to unmask]> 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: February 9, 2011 12:13 PM
To: [log in to unmask]
Subject: [TN] Thermal shock, IPC-TM-650 sec 2.6.8 ot 2.6.27

Folks,

   Given:
-        FR4
-       Th.  0.094 inch
-       Layer Count   20
-       Technology
o       4 tier totem pole stack micro vias
o       Buried conductive filled blind vias
-        Post 3x and 6x solder float test
-        Cross section

What are some of the expected anomaly to look for?

Victor,


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2