Greg,
I have used another method that is a bit messy, but non-destructive. I have
used this for checking actual temp of components during operation, but I
would think it would work for profiling also. Use some method to
strain-relieve the thermocouple wire, placing the actual thermocouple
junction on top of the area of interest, then use a dollop <sp?> of thermal
compound to fill any gap between the area of interest and the thermocouple
junction. This is a bit messy, but it does clean up with no detriment. It
also keeps airflow from affecting the measurement, and gives a good thermal
connection to the area of interest. Just one more method to add to your
list.
Thomas DeSmit
EDA Librarian/Sr. Engineering Tech.
IFR Americas, INC.
The opinions expressed are my own, and do not necessarily reflect those of
my employer.
> -----Original Message-----
> From: TechNet E-Mail Forum. Greg Jones <[log in to unmask]>
> [mailto:[log in to unmask]]
> Sent: Wednesday, October 14, 1998 9:03 AM
> To: [log in to unmask]
> Subject: [TN] Attaching Thermocouples for Profiling
>
>
> Good Morning Technet:
>
> Yesterday I inquired about methods other than soldering for attaching
> Thermocouples to PCB's for profiling. Thank you to those who responded.
>
> My list of quick and nondestructive methods now includes Kapton tape;
> Aluminum tape; Saunders Temprobes; and Loctite "TackPak". Are there any
> other methods or products I have missed? We're hoping to make our
> experiment as complete as possible.
>
> Thanks,
> Greg Jones
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|