Hechong -
As reported previously, there is no "one size fits all" for line width.? Previous post answered some of the electrical property and heat rise caluculations.?
From a fabrication standpoint, the critical parameter is "how thick is the copper of this layer"??? 3.5 mils is easy in 5 micron and 9 micron (0.2 and 0.35 mil foil).? It is OK in half ounce 17 micron (0.7 mil) foil.? Good shops can do it in one ounce 35 micron (1.35 mil foil).? It is state-of-the art in two ounce foil!!!
Then, are the traces inner or outer layer?? Inner layer typically have the best resolution as there is only photoresist and etching steps involved in fabrication.? Outer layers may have more copper plated and use a metallic plated etch resist instead of organic photoresist.?
One source of capabilty information is the PCQRR (Printed cricuit Capability, Quality, and Relative Reliability) team for IPC.? Their reports show all this against the best, good and average printed circuit fabricators.
Denny Fritz
MacDermid, Inc.
-----Original Message-----
From: Cong He <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, 16 Feb 2009 9:07 pm
Subject: [TN] PCB'S minimum line width
Hi all,
I want to know that how much is the minimum line with when you usually
designe the PCB?
The surface and the inner sides?
And what does that affect except the process capability of the PCB
factory?
Will 3.5mil be OK?
Hechong
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|