TECHNET Archives

June 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Andy Slade <[log in to unmask]>
Date:
Fri, 4 Jun 1999 08:13:57 -0400
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (74 lines)
     Nick,

     You need to determine the source of the discoloration and eliminate
     it.  Is it present right after immersion gold?  Could be poor rinsing
     or drying or both.  Do boards get soldermask before or after immersion
     gold?  If after, it could be mask or developer residue.  Are boards
     handled with bare hands or gloves after gold?  Should always handle
     immersion gold product with clean gloves, rack only, do not lay flat
     and slipsheet.

     A dip in a soap cleaner such as Morton's LAC-91 does wonders for
     cleaning up fingerprints and water stains from soft gold.  However,
     you must get a thorough rinse and sufficient drying or you just get
     more water stains after.

     Hope this helps...Andy


______________________________ Reply Separator _________________________________
Subject: [TN] Pad Discoloration???
Author:  Nick Liang <[log in to unmask]> at smtplink-hadco
Date:    06/04/99 11:17 AM


All:
One question about the Pad Discoloration Spec. (Immersion Gold pcs...)!!

I don't think the IPC has the Spec., right?
Is it required to use acid rising after the E/Test and FQC inspection???

You know, right now we just use the water rinse and 120mins baking
right after the Routing Process and then E/Test, FQC, OQC and Packing.

A lot of Pad Discoloration Quality Issue Feedback recent time!!!!

THKS.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2