Hello Folks!
A question for someone with knowledge of PWB laminant materials. I'm
sure IPC-4101 would tell me, but I don't have it.
If I've ordered material per IPC-4101/40, and have received material
per IPC-4101/41, is the /41 material:
a) the same material but tested to a higher standard?
b) better than but a different material?
c) worse than?
d) some combination of these?
I know the /40 is a polyimide material, I don't know what a /41 is.
Thanks!
regards,
Graham Collins
Process Engineer,
Northrop Grumman Canada Corporation
Halifax
(902) 873-2000 ext 6215
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|