Nitrogen reduces the oxide removal burden on the flux but also increases the
surface tension of the solder.
So there is no benefit from reducing oxide burden if you have a competent
flux in your solder paste, but the flux will have more work to do to
increase the wet out to overcome the increased coherent forces from the
solder.
Overall for tin lead reflow soldering it is hard to justify nitrogen.
In SAC lead free reflow any benefit from increased wetting is normally more
than out balanced by the further increase in surface tension (SACs have
higher surface tension then Sn/Pb). So overall the use of nitrogen in lead
free usually results in increased tombstoning, especially on smaller
devices.
The use of nitrogen injection in wave soldering to cut down drossing in wave
is 100% percent beneficial and even more so when lead free soldering.
Regards
Mike Fenner
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jerry Dengler
Sent: Monday, December 18, 2006 3:31 PM
To: [log in to unmask]
Subject: Re: [TN] Nitrogen usage
In a Sn/Pb environment (no experience with nitrogen in Pb-Free) I agree
with Rich. The nitrogen opens the process window but a good
manufacturer can build most assemblies just as well without the added
cost of nitrogen. That being said there are some designs that simply
will not give good yields without nitrogen.
Jerry Dengler
Production Manager
Pergamon Corporation
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Monday, December 18, 2006 2:51 PM
To: [log in to unmask]
Subject: Re: [TN] Nitrogen usage
To come down on the other side of this discussion....
I'd have to say that nitrogen is not necessary in all applications.
There is tendency to just through resources at the process saying that
it should be better (not arguing that it actually won't help!!).
Sure isn't nice and should help, but is it truly necessary in all
instances?
How much can it cost? To inert a high usage reflow oven for a year can
easily cost you ~$50K / year.
In today's world were every penny counts, it's another process parameter
that needs to be closely looked at and at least optimized.
Rich K / KEG
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Nowland, Russell
Howard (Russell)
Sent: Monday, December 18, 2006 2:13 PM
To: [log in to unmask]
Subject: Re: [TN] Nitrogen usage
John,
I am still waiting to get a quote back from them. We always used
nitrogen for just about everything and our previous EMS did too. This
is the first Tier 1 EMS I have worked with that did not.
Russell Nowland
Alcatel-Lucent
Supply Base Engineer
Address: 14000 Quail Spring Parkway, Suite 300 Oklahoma City, OK 73134
email: [log in to unmask]
Desk: 405-302-1660
Cell: 405-203-0034
Fax: 405-302-1622
-----Original Message-----
From: John Burke [mailto:[log in to unmask]]
Sent: Monday, December 18, 2006 12:35 PM
To: 'TechNet E-Mail Forum'; Nowland, Russell Howard (Russell)
Subject: RE: [TN] Nitrogen usage
I have had this issue too. All Tier 1 - 2 CM ovens are "nitrogen
capable".
I actually specified Nitrogen on the build requirements when I was
running manufacturing engineering at Extreme Networks and after a time
it was interesting the lengths that the CM would go to on "studies" to
try and persuade my upper management team that it could be switched
off!!!
There is some argument that can be applied to not using it, where for
instance the flux is a high activity system that is subsequently water
washed, but in general, the reality is, that the nitrogen reduces
oxidation of the soldering system and therefore improves the probability
of getting a "right first time" assembly with good probability of field
reliability.
What price are they talking about? The cost of the nitrogen? Or the cost
of the vacuum wall piping runs to take it into the factory?
I do not believe I have ever seen the specification that you refer to
(although I have sometimes wished there was one!)
John
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Russ Nowland
Sent: Monday, December 18, 2006 10:07 AM
To: [log in to unmask]
Subject: [TN] Nitrogen usage
Hello Technetter's,
Sometimes in life you find yourself in a pickle and wonder how the heck
you got there. It always brings me to that famous quote "It is hard to
soar with the eagles when you work with a bunch of turkeys".
I have a question: I am working with and "MAJOR" EMS that does not use
nitrogen with either Sn/Pb or Pb-free reflow. In this day and age I
have never heard of this. They have it available but will only use it
if I require it. At a price, of course. They don't seem to take into
account it will improve their yields as well.
Is there an IPC, NEMI, or any other standard that requires/recommends N2
usage for either Sn/Pb or Pb-free reflow process?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient please delete and
contact the sender by return and delete the material from any computer. Any
review, retransmission, dissemination or other use of, or taking of any
action in reliance upon, this information by persons or entities other than
the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. In particular, Indium
Corporation does not accept responsibility for changes made to this email
after it was sent. Any opinions or recommendations expressed herein are
solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient please delete and
contact the sender by return and delete the material from any computer. Any
review, retransmission, dissemination or other use of, or taking of any
action in reliance upon, this information by persons or entities other than
the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. In particular, Indium
Corporation does not accept responsibility for changes made to this email
after it was sent. Any opinions or recommendations expressed herein are
solely those of the author. They may be subject to change without notice.***
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|