Agree with Steve,
we mount thousands of resonators, different kinds, size and purpose. Other tips are:
-dewetting, have a look at the resonator's finish
-gas bubbles that can't escape, causing faint solder joints
-no wetting, make globule test or similar
-insufficient solder
-shaky soldering, disturbs solidification
-puck to heavy, does not let in flux and correct process,make small distance
not easy to say more without an idea of your situation.
Last chance: ask Paul Klasek, but you need a decrypting machine (he-he)
Ingemar
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: den 24 februari 2000 19:45
To: [log in to unmask]
Subject: Re: [TN] Resonator soldering problem
In a message dated 02/24/2000 12:26:51 PM Central Standard Time,
[log in to unmask] writes:
<< I have this Resonator part that is very large and sets on the top of the
PCB and
goes through our convection reflow oven at 220 C. Board is very complex and
the
problem we are having is that only the edges are being soldered and when we
cross-section to inspect solder under part it is still uncured. We discovered
this problem when parts started falling off PCB.
Any and all comments welcomed. What we would like to know is if any one else
is
using this part and have they solved this problem..
Steve >>
Hi Steve!
Can you tell us a little more about this part? I mean how large is very
large? Is it a ceramic part? Also when you say the board is going through the
oven at 220º C., where exactly is that temperature measured on the board?
What kind of solder alloy are you using...a 63/37? If so, then if the
resonator location is seeing 220º C., there should be no problem. Sounds to
me like a good temperature profile plot needs to be done with a thermocouple
placed at the resonator terminals...seems to me that there's not enough
calories to reflow the solder...
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|