TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Martin Butcher <[log in to unmask]>
Date:
Mon, 27 Jun 2005 14:08:46 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=ISO-8859-1
Subject:
From:
Bruce D Stilmack <[log in to unmask]>
In-Reply-To:
Content-transfer-encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (117 lines)
I agree, we use Dymax UV cure for most of our CCA assembly needs.

Bruce Stilmack
GDLS-TO Manufacturing Engineer
(850) 574-4773
[log in to unmask]


                                                                       
             Martin Butcher                                            
             <mbutcher@APEXMIC                                         
             ROMFG.COM>                                                 To
             Sent by: TechNet          [log in to unmask]                 
             <[log in to unmask]>                                          cc
                                                                       
                                                                   Subject
             06/27/2005 01:24          Re: [TN] Light Cure Adhesives   
             PM                                                        
                                                                       
                                                                       
             Please respond to                                         
              TechNet E-Mail                                           
                   Forum                                               
             <[log in to unmask]>                                         
             ; Please respond                                          
                    to                                                 
              Martin Butcher                                           
             <mbutcher@APEXMIC                                         
                ROMFG.COM>                                             
                                                                       
                                                                       




You might try Dymax.  They have been helpful in the past.

-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Monday, June 27, 2005 10:03 AM
To: [log in to unmask]
Subject: [TN] Light Cure Adhesives


Our current adhesive of choice is RTV.  Unfortunately it has a long cure
time and may be banned from use in products going to the European Union in
the coming years.

Our application is bonding 4 capacitors together.  The adhesive needs to be
thick (medium to high viscosity) so it won't sag, drip or run before
curing.
UV cure would be best from a time standpoint.  A "glob" of about 1/4"
should
be about right for this bonding application.  The capacitors have an epoxy
coating and the operating temperature is about 50° C maximum submerged in a
dielectric oil.  Electrical or thermal conductivity is not needed.  Method
of application is expected to be via small air actuated syringe or similar.

Anyone want to put in their 2¢?

Sales calls offline please.

Phil Nutting
Design for Manufacturing Engineer
Kaiser Systems, Inc.
126 Sohier Road
Beverly, MA 01915
voice: 978-922-9300 x1310
fax: 978-922-8374
e-mail: [log in to unmask] <mailto:[log in to unmask]>
www.kaisersystems.com <http://www.kaisersystems.com/>



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




This is an e-mail from General Dynamics Land Systems. It is for the intended recipient only and may contain confidential and privileged information.  No one else may read, print, store, copy, forward or act in reliance on it or its attachments.  If you are not the intended recipient, please return this message to the sender and delete the message and any attachments from your computer. Your cooperation is appreciated.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2