TECHNET Archives

January 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 21 Jan 2009 22:21:38 +0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, jonathan noquil <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=ISO-8859-1
From:
jonathan noquil <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Hi techies:
Does anybody from here had an experience on UMICORE solder paste?
I am using 95/5Sn from UMICORE and they claim it as no clean flux. However
residues are teribble.
I have problem on removing these residues. The flux residue is dark some
sort of it is burned or charred. And really difficult to remove during flux
cleaning using Ionox 1332?
I encountered lots of wirebond non-sticks.

Is this normal to UMICORE/Microbond pastes?

Hope to hear from all of you.

regards
Jon

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2