Scott,

Many of the other large shops that run liquid resists have encountered the
same types of problems.  Often the resist supplier will promote the resist as
a product that can be stripped with caustic, without thought to bath life,
particle size, and copper appearance for AOI.

In response to this, we have developed specific strippers for the various
liquid resists.  We have engineered them to have a non-sticky particle that is
large enough be filtered with a large mesh, yet small enough to transport
efficiently through the filtration unit.  The strippers tend to be very long
lasting because of the high efficiency of the filtration (1200+ MSF), and they
all have an antitarnish package to keep the layers clean for days in AOI.

Please let me know what resist you are using, and I'd be glad to send more
specific information to you, or our distributor (Great Western) can drop off
the information.

Additionally, if you would like, I can get you references at JME/ACI, and/or
Via Systems on their experiences with liquid resists and stripping.

Sincerely,
Scott Griggs
Chemelex Division of RBP Chemical Corp.
(612) 825-6113
[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2