In the US Many Precious metals Companies Will take the PWB units off your
hands for nothing and smelt them down for the metal content. We would look
up in a local telephone book for companies that will perform this type of
reclaim.
Also, Hirsch Metals may be interested:
Hirsch Metals Corporation
4733 West Atlantic Avenue
Building C Suite 12
Delray Beach FL 33445
Tel: 561-638-3400
Fax: 561 638 3444
[log in to unmask]
I guarantee there are people willing to remove these PWB's for you.
Best Regards,
Cal Driscoll
Communications Test Design, Inc.
www.CTDI.com
-----Original Message-----
From: Bissonnette, Jean-Francois [mailto:[log in to unmask]]
Sent: Monday, June 09, 2003 10:52 AM
To: [log in to unmask]
Subject: [TN] PWB disposal
Hi all,
We have to dispose of over 300lbs of PWB. Before putting everything in a
garbage can, I was wondering if
there was any specific way of disposing of circuit boards (environnemental
concerns).
Jean-François Bissonnette
Vérificateur, Contrôle de la Qualité
Électronique
Produits et Procédés
Vapor Rail Inc.
10655 Henri-Bourassa O.
St-Laurent, Qc
H4S 1A1
(514) 335-4200 x2021
(514) 335-4231 fax
***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged and
confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|