At the last IPC EXPO, I presented a paper that mathematically models the
electroplating process for through holes using the Navia Stokes equations
for fluid flow and Faraday's law for electroplating . The parameters of
first order importance which were identified by this analysis are (hole
diameter/aspect ratio)-squared (not aspect ratio alone), current density,
concentration and agitation speed. Unfortunately, most of these parameters
suggest that improvements in the hole wall uniformity require additional
expense. As we all know, improved reliability, often requires a more
expensive process.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|