TECHNET Archives

December 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jean-Francois Bissonnette <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 15 Dec 1999 11:39:27 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (41 lines)
Hello technetters!

Well thank You for your enthousiastic answers concerning
your identities.  I'll give you some details about my
occupations ounce I get rid of some fires here (it's funny,
nobody mentioned firefighter!!!).

Some people here are getting pretty nervous about one
IPC-A-610 criteria here and honestly I dont know what
what to tell them to ease their worries.

Par. 3.2.4 says that class 1 & 2 permits coating meniscus
of capacitor to be mounted into PTH.  But is'nt there a
risk of preventing the solder to be conform to criteria
4.1 table 1 (saying that the solder must fill 75% of
the hole)?  What is the risk of not respecting this criteria
(3.2.4).  Personnaly I would fear craquing for the capacitor
on the long run (plus the solder fill), this thing will be submit
to constant vibrations (It goes on a train, near the braking system).
So I would prefer to have it above the meniscus.  But here they
are concerned with the overall costing... Well I guess I need
some of these 5000 years of experience now!

Thank You!  See you around!

JF

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2