The Eutectic temp is the lowest temp at which melting is seen with a
eutectic composition
of different (or all the same) elements say tin(Sn) and lead(Pb). At a one
composition of tin & lead there is one temp that both elements (alpha & Beat
regions of each element) will start to be liquid.
Basically a particular percentage of each part at a particular temp will all
start to be liguid. That is the eutectic temp.
I hope I expalined this clear, correct, and simple enough.
Bob Wolfe
> -----Original Message-----
> From: Lon Weffers [SMTP:[log in to unmask]]
> Sent: Tuesday, April 25, 2000 3:24 PM
> To: [log in to unmask]
> Subject: [TN] eutectic
>
>
> Dear friends,
>
> It might seem a stupid question, but what does Eutectic mean when they
> talk
> about eutectic soldertemperature?
>
> Thanks in advance
> Lon weffers
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|