TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Charles Barker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 21 Feb 2000 10:59:45 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (131 lines)
Hi Brian,

Thanks for the input. No, we will not short-circuit all evaluations... Aside
from reading the data sheets, I hope to use this information to drastically
narrow down which brands and models we look at and what we test on each one.

Folks who have already run a "stencil abandon time" test, for instance, can save
us a bunch of time and energy if their equipment and environment is similat to
ours. Applications specific to our products and processes will still need to be
checked out.

Thanks for the feedback.

Charlie B.



Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
      Brian Ellis <[log in to unmask]>








 To:      [log in to unmask]

 cc:      (bcc: Charles Barker/US/I-O INC)



 Subject: Re: [TN] THANKS and no clean info request








Charlie

Welcome back.

I'm sure several responses may help you but, before you short-circuit
all evaluation, please remember the two basic facts:

1. Water-soluble chemistry gives you the widest operating window
2. "No-clean" chemistry gives you a narrow operating window.

This means that it is really impossible to just switch, as there are so
many parameters to consider, e.g. solderability of boards and
components, desired reliability of end product etc., etc., etc. Another
point that it is important to realise: the term "no-clean" covers a
multitude of sins and the easiest "no-clean" fluxes/pastes to use are
those which are the most active and may leave the most active residues,
causing future problems.

I would therefore counsel caution in interpreting the responses to your
enquiry. Caveat emptor.

Brian

Charles Barker wrote:
>
> Hello Technetters;
>
> As Steve Gregory let slip last week, I am back on the job. I'm somewhat
> inundated with catching up, so I had not checked back in on TechNet right
away.
>
> MANY THANKS for all the prayers and good wishes. They were felt and very much
> appreciated by both my wife and me. I still have a good bit or soreness from
the
> trauma of the surgery, but in general, I feel very good.
>
> Now back to the work/no clean thing:
>
> I am asking a BIGGG favor!
>
> I need to take a serious look at switching our process from a water soluble
flux
> soldering operation to a no clean one. Normally, I would put several cored
wire
> solders, liquid fluxes and solder pastes through a rigorous evaluation
process.
> That could be considered re-inventing the wheel, since many of you have
probably
> already done that.
>
> If any of you have done this and could share the results (OFF-LINE, of
course),
> I would be greatly obliged.
>
> I would like to know which brands, which model numbers, which alloys and under
> what conditions they were tested, as well, of course, as the results.
>
> THANKS A BUNCH!!!
>
> Charlie B.
> [log in to unmask]
>

--
Brian Ellis
Protonique SA
PO Box 78
CH-1032 Romanel-sur-Lausanne, Switzerland
Voice: +41 21-648 23 34 Fax: +41 21-648 24 11
E-mail: [log in to unmask]
URL: Technical and consultancy divisions:
       http://www.protonique.com
     Web services division:
       http://www.protonique.com/webserv

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2