Dear Ms. Nguyen:
The test method employed is described in IPC TM-650, 2.6.3.3 as referenced in Joint Industry
Standard J-STD-004 "Requirements for Soldering Fluxes". I would recommend contacting Mr. Jim
Hevel at SCOPE LABORATORIES, 708-335-8888.
Regards,
Ted Stern
My Nguyen wrote:
> Hello,
>
> We are changing the post-reflow washing window from 1
> hour to 5 hours. However, in order to do it, we have
> to provide proof to our customer. One of the
> requirement is the SIR.
>
> Could you please show me what tool do I need and where
> to buy to do the SIR test. What is the most
> popular/approriate procedure to do it?
>
> Your help is greatly appreciated.
>
> Thanks,
>
> Stacy
>
> __________________________________________________
> Do You Yahoo!?
> Send your FREE holiday greetings online!
> http://greetings.yahoo.com
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|