TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Maguire, James F" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 6 Apr 1999 11:09:21 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (82 lines)
Ed,

We actually did thermal shock testing of untinned LCCs (ceramic parts, right) on controlled CTE PWAs (best case) to try to determine how "bad" not tinning was.  Answer:  It was bad.  Most parts failed at <100 cycles (normal parts were ~1000 cycles).  We often go around on this (typically 1-2 parts per year we "just can't tin" and we re-visit this issue).  We've always gone to tinning, even as far as recalling hardware to do it.  Note that the Au "limit" is ~4% by weight (~1.8% by volume in Sn63); beyond that is BAD.).  Also note that just a gross volume calculation (Au vs. Solder volume) can be misleading as the Au doesn't always evenly distribute in solder, it's the locallized concentrations that kill ya.

I have some detailed info (too large to Technet) but if you can accept ~1 meg inputs I can mail to you.  Let me know.

Jim
---------------------------------------------------------
Jim Maguire
Boeing Phantom Works
E/E M&P
Phone (253)657-9063
fax       (253)657-8903
Pager  (206)982-3737
email:  [log in to unmask]
---------------------------------------------------------

> ----------
> From:         Knowles, Ed[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;Knowles, Ed
> Sent:         Monday, April 05, 1999 2:28 PM
> To:   [log in to unmask]
> Subject:      [TN] Gold Embrittlement
>
> Please don't blast me on bringing this subject up again.  I have searched
> the TechNet archives and found lots of good information, and also noted that
> it is a somewhat sensitive subject, having been around for 30+ years.  We
> have a condition that I believe is clearly unreliable based on what I have
> read.  The condition is:
>
> - 4 lead LCCC's (leadless with castellations)
> - Approximately 50 microinches of glod plating on untinned castellations.
> - Untinned parts mass reflow soldered onto PWB's (parts were supplied on
> tape and reel, so subcontractors did not see that they were untinned).
> - Microsectioning shows a 50 to 100 microinch layer of Au/Sn intermetallic
> after soldering, on top of copper/nickel surface.  Au concentration averages
> about 25% in this intermetallic region.
> - These assemblies will be subjected to high vibration and long term (years)
> thermal cycling in actual use.
>
> Replacement of these parts would be expensive since they are on many boards
> installed in closed and tested boxes. For this reason, mangement is hoping
> that testing will qualify this condition.  I hate to see the affected
> program waste time and money, and am afraid they might even get a warm fuzzy
> and fly these parts.
>
> Can any of the numerous industry experts in this group give me something
> concrete to present to the program such as actual experiences or obtainable
> reports?  Is the above condition a no-brainer or is it not as bad as it
> looks to me?  I tried getting copies of the 2 reports listed in the
> J-STD-001 Handbook, but struck out.
>
> Thank you for your time.
>
> Ed Knowles
> Lockheed Martin
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2