Frank,
Try the National Semiconductor web site. They provide free slide rule type calculators for transmission line calculations including edge coupled. Also, if you have the cash to spend, Polar Instruments has software that will do the same.
Rick
-----Original Message-----
From: F. D. Bossert [mailto:[log in to unmask]]
Sent: Wednesday, October 06, 1999 10:09 AM
To: [log in to unmask]
Subject: [TN] Impedance Calculation
Sirs,
Does anyone have a impedance formula for "Edge coupled surface microstrip"?
Any help would be appriciated.
Thanks
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|