Joseph,

The first three items are easy.  Its the "inexpensive" that trips us up.

Here are some suggestions.

3M #42, Anti-static Kapton tape, solder mask  (This is our standard wave
solder mask for edge connectors and large holes.)

3M #5419, Anti-static Kapton tape, solder mask (has a sticker adhesive)

3M #5413, Kapton but not anti-static

3M #5414, polyvinyl alcohol backing which is water soluble and a synthetic
water soluble adhesive designed to mask gold fingers during wave solder.

Then there is 3M #219, a high performance green film backed tape, designed
for conformal coating masking with a working temp of 275°F but not listed as
anti-static.

Hope this helps,

Phil Nutting
Manufacturing Engineer
Kaiser Systems, Inc.

-----Original Message-----
From: Kane, Joseph [mailto:[log in to unmask]]
Sent: Friday, December 01, 2000 9:43 AM
To: [log in to unmask]
Subject: [TN] Conformal Coat Masking


Can anyone out there recommend a good masking tape?

Desired properties, in approximate order of importance:
1. Withstands 85C indefinitely.
2. Sticks well, but peels off without leaving residue.
3. Antistatic a plus, but conductive probably not worth it (we
    use ionizing air blowers).
4. Inexpensive.

Our coatings are mostly urethanes, manually sprayed.

Joe Kane
BAE SYSTEMS Controls
Johnson City, NY

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2