TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
X-To:
Steve Collins <[log in to unmask]>
Date:
Thu, 14 Aug 1997 09:03:52 -0700
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Delsen Testing Laboratories <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Delsen Testing Laboratories <[log in to unmask]>
Parts/Attachments:
text/plain (18 lines)
Steve,

Try IPC-ET-652 "Guidelines and Requirements for Electrical Testing of Unpopulated
Printed Boards".  I'm sure it's available from the IPC.

Brian McCrory
Chairman, IPC Testing Committee

Delsen Testing Laboratories, Inc.
1024 Grand Central Ave.
Glendale,  CA  91201

Phone:  818 247 4106
FAX     818 247 4537
email:  [log in to unmask]
URL:    http://www.primenet.com/~delsen/