TECHNET Archives

1995

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0tJp87-000104C; Sun, 26 Nov 95 16:00 CST
Old-Return-Path:
<miso!compuserve.com!100760.351>
Date:
23 Nov 95 19:07:31 EST
Precedence:
list
X-Loop:
Resent-Sender:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/249
From [log in to unmask] Sat Apr 27 15:
20:56 1996
TO:
Return-Path:
Resent-Message-ID:
<"ZkRZ-1.0.mDA.QEEkm"@ipc>
Subject:
From:
Michael Fenner <[log in to unmask]>
Message-ID:
Resent-From:
Parts/Attachments:
text/plain (24 lines)
If the problem you have is ingress or retention of moisture (and associated
ionics) then no semi-aqueous process is going to be satisfactory as these
involve a water rinse. Some of the glycolether products aka oxygenated alcohols
- Prozone Dowanol Zestron etc- can be used solvent/solvent instead of
solvent/water, in addition some people use  isopropanol instead of water. You
would have to take account of the flammability of the IPA before going down this
route. 
Mike Fenner
Bonding Services UK
[log in to unmask] 
--------------------------------------
 We are currently using Duriod 6002/6010 type PWB's on one of
          our products and are having problems cleaning the PWB's
          after soldering and assembly operations.  Removal of fluxes
          and the cleaning fluid (Axarel) from this very hygroscopic
          material has been difficult inspite of using the
          Manufacturers recommended process.  Any information
          or sources of potential information relating to resolving
          this situation would be appreciated.