And Valerie, that was a lot of good input.
I just wish some sort of standard for pwb reliability could be agreed on
beforehand, to eliminate all of the lawsuits, etc.
No one is considering the fact that because some boards may be intended
for standard 63/37 solder processes, but contain BGAs with Pb-free
solder balls, the industry will need to increase the temp. somewhat, as
was described last week. But the circuit boards can barely withstand
current standard processes. Will they be able to withstand an increase
in process temperatures to accomodate the Pb-free BGAs, at around 230
deg. C?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Tuesday, December 13, 2005 12:28 PM
To: [log in to unmask]
Subject: Re: [TN] Qualification of the Pb-free capable manufacturers
Hi Valerie,
AMEN to all of that---and PLEASE do not hold your breath waiting for
this to happen anytime soon.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|