TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"McGlaughlin, Jeffrey A" <[log in to unmask]>
Date:
Mon, 6 Nov 2000 09:57:52 -0500
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "McGlaughlin, Jeffrey A" <[log in to unmask]>
Parts/Attachments:
text/plain (116 lines)
James,

The only reason I can think of for specifying core construction over foil
construction is if you have controlled impedance traces, or an need for
tightly controlled dielectric spacing for outer layer to first internal
plane layer.

Otherwise the advantages of foil construction include better layer to layer
alignment (fewer features to align) and more control of outer layer copper
before plating (fewer passes through cleaning/stripping process).

Jeffrey A. McGlaughlin, C.I.D.
Sr. PCB Designer
Battelle Memorial Institute
Columbus Ohio
[log in to unmask]


-----Original Message-----
From: Roger M. Stoops [mailto:[log in to unmask]]
Sent: Monday, November 06, 2000 9:10 AM
To: [log in to unmask]
Subject: Re: [TN] MULTILAYER BOARD LAY-UP


James,
What your vendor is proposing is the foil construction method of PWBs vs.
core construction.  For some vendors, foil construction saves a little
money, provides easier manufacturing (fewer innerlayer cores to process),
reduces warpage, and possibly a few other benefits one of the fab gurus
could comment on..  In the end you have the same, but possibly better,
board.  Most of our boards are foil construction, and we have seen no
problems with this form of PWB construction.
Roger M. Stoops, C.I.D., PCB Designer


Spectra Precision Inc./Trimble Navigation Ltd.
5475 Kellenburger Rd.
Dayton, OH 45424-1099 USA
Ph: 937.233.8921 or 937.233.4574 ext 288
Fax: 937.233.7511



                    "Marsico, James"
                    <James.Marsico@D        To:     [log in to unmask]
                    P.AIL.COM>              cc:
                    Sent by: TechNet        Subject:     [TN] MULTILAYER
BOARD LAY-UP
                    <[log in to unmask]
                    >


                    11/06/00 08:21
                    AM
                    Please respond
                    to "TechNet
                    E-Mail Forum.";
                    Please respond
                    to "Marsico,
                    James"





Dear Techneters:

I have a six-layer board design which requires three polyimide cores bonded
together with two layers of prepreg.  Our PWB supplier is recommending
using
two cores bonded together with prepreg, then bonding copper foil on both
outside layers also using prepreg.  The resultant dielectric thickness'
would remain similar to the original design.  Are there any drawbacks to
this approach?  What is the benefit?

Thanks,
Jim M.

----------------------------------------------------------------------------
-----

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2