TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Genny Gibbard <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Date:
Wed, 13 Apr 2005 13:52:08 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (54 lines)
You need to look at the technet Archives.  Steve G posted adetailed account
of emptying a pot about 2-3 years ago.
Try this:
http://listserv.ipc.org/scripts/wa.exe?A2=ind0209&L=technet&P=R5161&I=-3
I don't think the pics are still available, unless Steve would like to put
them back up on his site.

-----Original Message-----
From: Anderson, Greg (GE Infrastructure)
[mailto:[log in to unmask]]
Sent: 13-Apr-05 1:27 PM
To: [log in to unmask]
Subject: [TN] Wave Solder Pot Draining Best Practices


TechNet:

We are going to drain and clean a wave solder pot in preparation for
conversion to lead-free solder.

We have not completely purged a wave solder pot in some time, and the people
in the know have moved on.

Does anyone have "best practices" recommendations for draining and handling
the solder (other than BE VERY CAREFUL ! ) ?

Greg Anderson
GE Fanuc Automation
Charlottesville, VA

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2