Peter,
Have you considered the possibility of the solder resist being damaged
during
the solder wicking of the pads before placing the replacement package. This
can make placing and getting good reflowed devices extremely anoying!
Also, might seem like a strange one, but I have seen what looks to be a
short on an x-ray which is actually intentional if you look at your gerber
files
where the two balls are for instance at ground etc ...
Regards,
Doug McCall
PCB Manufacturing Engineer - Eastbourne
BOC EDWARDS
Marshall Road,
Eastbourne,
East Sussex,
BN22 9BA UK
' +44 (0) 1323 501 147
7 +44 (0) 1323 509 824
* [log in to unmask]
BOC Edwards is a part of BOC Limited
Registered Office: Chertsey Road, Windlesham, Surrey GU20 6HJ
Number 337663-English Register
Ultimate holding company: The BOC Group plc
-----Original Message-----
From: Peter Lee [SMTP:[log in to unmask]]
Sent: 09 September 2002 21:16
To: [log in to unmask]
Subject: [TN] BGA rework - excessive collapsing
Technet,
We are having problems replacing 35mm BGA, 1.27mm pitch on a OK
industry
BGA rework station. The resulting X-ray revealed a solder bridge at
one
corner.
There was some warpage on the BGA but not significant. PCB was
reasonably flat. Thermal profiling was done to ensure all temp. were
optimum. I did notice the BGA balls collapsing quite a bit (at least
half of the ball height) after rework.
Anyone has suggestion on how to minimize the chance of bridging? Is
it
common for BGA of this size? We don't have the capability to paste
the
board for BGA rework.
Rgds,
Peter
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
_____________________________________________________________________
This e-mail has been scanned for viruses by the WorldCom Internet
Managed Scanning Service - powered by MessageLabs. For further information
visit http://www.worldcom.com
_____________________________________________________________________
This e-mail has been scanned for viruses by the WorldCom Internet Managed Scanning Service - powered by MessageLabs. For further information visit http://www.worldcom.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|