TECHNET Archives

August 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 13 Aug 2015 15:14:35 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
<00e801d0d5d2$621dc130$26594390$@[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Jonathan Griffiths <[log in to unmask]>
X-cc:
Thomas Jones Merlin Circuit Technology Ltd <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (124 lines)
Not sure if this completely relevant..

We have been working with researchers in the UK, at Leicester university and they have developed a new, cheap, non-toxic, ionic-liquid flux.

Using this flux they have successfully soldered directly onto oxidised Nickel as well as oxidised Copper surfaces. 

A new surface finish they are looking to develop with this flux is the HASLEN (Hot-air Solder Levelled Electroless Nickel), which is a next generation replacement to the standard HASL finish. 

For more information see (http://pcb.iconnect007.com/index.php/article/89160/haslen-a-new-high-reliability-surface-finish-for-pcbs/89163/?skin=pcb)
Contact details ([log in to unmask])"

Jonathan Griffiths
Quality Manager
Merlin Circuit Technology Ltd
Merlin PCB Group
E: [log in to unmask] 
DD: 01244 525 760
Explore The Merlin PCB Group companies at 
www.merlinpcbgroup.com
 
 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: 13 August 2015 15:04
To: [log in to unmask]
Subject: Re: [TN] Solderable Nickel?

Nickel is quite soluble in solder if not oxidized. There are many methods of preventing oxidation, including immersion gold plating (standard ENIG), OSP, and other organic or polymer coatings that are pre-stripped just prior to processing. This is very common.
I am just clarifying this for those who may not understand this thread because your emails seem to indicate that nickel is not solderable, period.
While nickel's rate of dissolution into molten solder is much slower than copper, silver, or gold, it is still quite solderable if not oxidized, and must be protected.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: Thursday, August 13, 2015 8:06 AM
To: [log in to unmask]
Subject: Re: [TN] Solderable Nickel?

We are on the same wavelength then:-). In essence, everyone literally solder either to Cu or your Ni.

There are only two ways of soldering to Ni I can think of: either have a rather strong flux (as you pointed out), or have something like "OSP" preserving its surface. ‎I've never heard of such thing though but it doesn't mean it can not exist.


Regards,

Vladimir
Sent from my BlackBerry 10 smartphone on the Rogers network.
  Original Message
From: David Hillman
Sent: Thursday, August 13, 2015 08:53
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: Re: [TN] Solderable Nickel?

Hi Vlad - let's characterize nickel this way: in general, nickel is solderable with the aggressive fluxes. The majority of the flux formulations used by many of the High Performance OEMs are ROL0 materials which traditionally were not very compatible with nickel surface finishes.
The flux formulations being used are not aggressive. So I have the some question as Ben - what's different about these new "solderable nickel"
surface finishes? I have subjected them to 150C bake for 4 hours and they meet the IPC-JSTD-002 testing criteria. Pretty impressive.

Dave

On Thu, Aug 13, 2015 at 7:27 AM, Vladimir Igoshev < [log in to unmask]> wrote:

> Ni in general is solderable. The clues to on is "for how long"! Are 
> you sure the parts font have a thin layer of Sn over Ni?
>
> ‎Regards,
>
> Vladimit
>
> Sent from my BlackBerry 10 smartphone on the Rogers network.
> Original Message
> From: Gumpert, Ben
> Sent: Thursday, August 13, 2015 07:35
> To: [log in to unmask]
> Reply To: TechNet E-Mail Forum
> Subject: [TN] Solderable Nickel?
>
> TechNetters,
>
> I've received several components recently that were plated with 
> 'solderable nickel' and to my surprise they soldered just fine (using 
> a
> ROL0 flux).
> Anyone know what is going on to keep the nickel from oxidizing?
>
> Ben
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


Export Control and ITAR regulations require customers to advise their suppliers if the product they have been asked to quote for or manufacture is subject to Export Control and ITAR regulations. If no mention of Export Control and ITAR appears on the quote request or order confirmation Merlin PCB Group companies are within their rights to assume that Export Control and ITAR regulations do not apply
Disclaimer: This email is confidential and may be privileged. If you are not the intended recipient please notify the sender immediately and delete the email from your computer. You should not copy the email, use it for any purpose or disclose its contents to any other person.  Please note that any views or opinions presented in this email may be personal to the author and do not necessarily represent the views or opinions of The Merlin PCB Group or companies within it. It is the responsibility of the recipient to check this email for the presence of viruses and we accept no liability for any damage caused by any virus transmitted by this email.



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2