TECHNET Archives

April 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
fgolisan <[log in to unmask]>
Date:
Thu, 30 Apr 1998 12:24:44 PST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, fgolisan <[log in to unmask]>
Parts/Attachments:
text/plain (85 lines)
     Setve,

         Suggest you install mixed bed system on the inlet water to the
     looped. These bottles should be available on a use basis without a
     monthly charges. Regeneration charges on the city water are minimal.
     You may even consider adding a carbon filter.
         Have you checked the cost for regeneration and or replacement of
     the bottles in the loop. Don't let them surprise you later. I would
     also suggest that the bottles be configured fully redundant. Complete
     Operational and Standby streams.

     Good Luck,

     Fred Golisano


______________________________ Reply Separator _________________________________
Subject: [TN] ASSY: Closed Loop Water Treatment System
Author:  "TechNet E-Mail Forum." <[log in to unmask]>, at corp
Date:    4/30/98 11:35 AM


Hello All,

     I'm going to be getting a Trek Triton IV SMT cleaner with a integrated
water treatment system here in a couple of weeks, and I've got a question that
maybe somebody can answer.

     The onboard treatment system has a 1 cu.ft. Carbon and chelate bed, and
two 1.5 cu. ft. cation and anion beds (so you can keep running while changing
one set when needed). We're just starting-up, so it'll be a little while
anyway before we start cleaning any serious board feet of printed circuit
boards.

      My question is; should I get rental DI columns to fill my cleaner, and
provide make-up water for the evaporation that happens during operation? Trek
says that I'll lose anywhere from 3-10 gallons an hour during normal
operation. They also provide a service that I send them a sample of the tap
water we have here and they'll do an analysis to get an idea of how hard the
water is.

     I was thinking that there has to be somebody from the S.F. bay area
that's already done this drill before, and knows if I need to rent additional
mixed-beds besides the ones that I have in the treatment system...the water is
the same all over the area here because we all get our water from the Hetch
Hetchy reservoir...

    I've always had rental beds at other places I've worked at here in "silly-
con" valley, but then we were talking 2-4 cleaners at a time and high-volume
work...this time it's only one cleaner, and I'm just trying to be "frugal".

     I was just going to run without a rental bed and monitor things to see
how it goes, but I don't want to kill my beds right away if there's a risk of
that.

                          Thanks in advance!!

                          -Steve Gregory-

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2