TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 6 Jan 2005 18:24:24 +0100
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Daan Terstegge <[log in to unmask]>
Subject:
MIME-Version:
1.0 (Generated by Clearswift ES version 4.8.1.149)
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
From:
Daan Terstegge <[log in to unmask]>
Parts/Attachments:
text/plain (77 lines)
Hello Alvin,

Lots of good info about HASL can be found via my website at
http://www.smtinfo.net
Just click on the link named "HASL".

Best Regards,

Daan Terstegge
PCB Assembly Department
Thales Land&Joint Systems

Tel:     +31(0)35 524 8297
Fax:    +31(0)35 524 8181
Unclassified Email



>>> [log in to unmask] 01/06/05 02:06am >>>
hi,

the full title of this msg is: "HASL (hot air solder levelling) solder
thickness impact on solderability with SnPb and Pb-free solder"

i am currently in my 3rd year in a local university in singapore. the
above
named issue is a project that i am supposed to do. due to my lack of
knowledge in this field, i would like to seek the opinions, advice or
help
from the people with expertise here.

the project objectives are as follows:

1) To study the extent of inter-metallic layer on thin HASL coating
thickness and the influence on assembly solderability.

2) To study any implication of lead free HASL as a surface finishing

3) To compare solderability of thick and thin HASL solder thickness
with
both SnPb and PB free solder

i would appreciate any facts, info or links to relevant
articles/reports/journals/magazines pertaining to my scope of the
project.
many thanks!

regards,
alvin

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2