We used to heat soak assemblies to be reworked for 2 hours at 90 deg C in a
calibrated oven, and re-heat them for half an hour after approx every 10
minutes of rework (if they took that long). Typically-used temperature ramp
rate for PCA's is 5 deg C/minute.
If you want to fine-tune the soak period to reduce the time in the oven,
stick a couple of thermocouples on the board attached to a data logger, and
see how long it takes for the board to reach the soak temperature.
Peter Duncan
"Rougeux, Scott"
<Scott.Rougeux@P To: [log in to unmask]
LEXUS.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST
Sent by: TechNet Aero/ST Group)
<[log in to unmask] Subject: [TN] FW: preheating assemblies prior
> to rework
09/27/01 03:21
AM
Please respond
to "TechNet
E-Mail Forum."
> Your input is requested on this issue.
> In regards to preheating assemblies prior to reworking them on the Solder
> Fountain/solderpot.
> We have been asked to look into preheating components or boards during
> rework. This opens many questions:
> * What is the desirable preheat temperature?
> * How is it measured?
> * Where is it measured?
> * How quickly can the assembly be heated?
> Thanks.
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|